江西预防环氧地坪漆失光

文章出处:本站 人气:19342 发表时间:2021-08-20 13:46:29

预防<a href=/art/cjwt28.html>环氧树脂<a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/pro/dpq26.html><a href=/art/cjwt95.html><a href=/art/cjwt95.html><a href=/art/cjwt95.html><a href=/art/cjwt95.html><a href=/art/cjwt95.html>地坪漆</a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a></a>失光

环氧地坪漆的施工技术和习惯是失光的重要原因之一,培养规范的施工技术和施工环境要求,按照规模的施工流程操作可以避免环氧地坪漆失光的概率。

施工现场湿度过高(相对湿度超过85%),挥发性涂料容易吸水发白。预防:施工现场湿度不宜过高。

被涂料表面过于粗糙或多孔,未涂封锁底漆会出现环氧地坪失光现象。这一原因造成的环氧地坪漆失光需要我们物面用底漆封住,腻子填平,打磨。

表面处理不干净,含有酸、碱、油、蜡、水。这就要求我们在施工前充分处理被涂层表面。

涂膜未完全干透前遇雨或露水。防止:涂膜在干燥过程中应防止雨水或露水浸润。

施工过程中稀释剂用量过多或加入煤油等高沸点稀释剂。预防:稀释剂用量不宜过多,应避免加入煤油等高沸点溶剂。

预防:应控制颜料的含水量,避免在施工过程中混入水分。

油漆中颜料含水量过高或施工中混有水分。

涂膜涂膜柔软,抗划伤性能差。预防:根据涂层的使用前提,选择耐候性和抗划伤性能好的涂层。